空泡腐蚀
- 网络cavitation erosion;Cavitation corrosion
-
TIG表面重熔对堆焊层耐空泡腐蚀的影响
Effect of TIG surface remelting process on cavitation erosion resistance for a pre-weld buildup layer
-
通过与传统磨削表面加工对比,研究了TIG表面重熔对空泡腐蚀的影响。
Compared with the conventional post grinding process for the weld layer , the effect of TIG surface remelting process on cavitation erosion resistance was investigated .
-
结果表明:在45h空泡腐蚀试验后,磨削试样的累积失重量是TIG表面重熔试样的1.57倍;
The results show that after 45h of cavitation erosion test , the mass loss of the specimen with ground surface was 1.57 times of that with TIG remelted surface .
-
双相不锈钢的磨损腐蚀与空泡腐蚀研究进展
Research Progress on Erosion-corrosion and Cavitation Erosion of Duplex Stainless Steel
-
水合肼溶液的化学腐蚀又加剧了空泡腐蚀。
The chemical corrosion by the hydrazine hydrate solution enhances cavitation corrosion .
-
湍流与空泡腐蚀,加剧了焊缝腐蚀的发展。
Rushing waters and cavitation corrosion aggravated the development of welding corrosion .
-
螺旋桨材料空泡腐蚀机理的扫描电镜研究
Investigation on cavitation mechanism of propeller materials by means of scanning electron microscope
-
一种钴基合金的空泡腐蚀行为研究
Cavitation behavior of a Co-base alloy
-
随着内燃机强载度的提高,内燃机冷却系统的管路、水泵、特别是湿式气缸套,常常存在穴蚀(又称空泡腐蚀和气蚀)现象。
With the increase of ICE output power , cavitation usually occurs in the pipe , water pump , and wet cylinder liner .
-
叙述了水合肼蒸发器加热管的腐蚀情况与腐蚀特征,分析其腐蚀原因主要是空泡腐蚀。
This paper describes the corrosion behavior of heating pipe in hydrazine hydrate evaporator , and shows that the main mechanism is cavitation corrosion .
-
通过讨论海上石油钻井平台用管材空泡腐蚀失效的案例,研究管材空泡腐蚀的宏观特征和微观特征。
The macro and micro characteristics of vacuolar corrosion were studied ; a failure case of vacuolar corrosion of petroleum pipe of seashore well-drilling rig was discussed .
-
采用空泡腐蚀与定位跟踪观察交替进行的方式,研究了灰口铸铁在自来水中空泡腐蚀过程的表面形貌演变。
The surface morphology progression of grey cast iron due to cavitation erosion induced by tap water has been studied carefully by cavitation corrosion test and SEM observation in turn .