  1. Microstructure and Properties of Vacuum Pulse-Nitrided layer of H13 、 3Cr2W8V Mould Steel

    H13、3Cr2W8V模具钢真空脉冲渗氮层的显微结构和性能

  2. This essay has analysed the process of heat-treatment of steel ( 3Cr2W8V ) mould and the cause of losing efficacy of mould severance . By improving the heat-treating technology , the mould life has been prolonged in a big range .