The results show that after 45h of cavitation erosion test , the mass loss of the specimen with ground surface was 1.57 times of that with TIG remelted surface .
结果表明:在45h空泡腐蚀试验后,磨削试样的累积失重量是TIG表面重熔试样的1.57倍;
-
Specimens cut from turbine disks of a Ni-Cr-Ti type wrought superalloy were heat treated for 29h and 45h at 980 ℃, the high-peak temperature of η - phase precipitation , so as to obtain various η - phase contents .
将从Ni-Cr-Ti型合金涡轮盘上切取的试样在该合金的η相析出峰值温度(980℃)热处理29h和45h,得到含不同η相数量的试样,测试性能。
-