环烷酸镍

  • 网络Nickel naphthenate;NiNaph
环烷酸镍环烷酸镍
  1. 催化剂的最佳陈化方式为:于50℃将HMPA加入到环烷酸镍(简称Ni)中,使其充分络合,然后加入三异丁基铝(简称Al)。

    The good catalyst preparation method was adding HMPA to nickel naphthenate ( Ni ) and stirring completely , and then adding triisobutlyaluminum ( Al ) at 50 ℃ .

  2. 空气-氩气冷却ICP-AES测定环烷酸镍中的镍、铁、镁和钙

    Determination of Elements in Nickel Naphthenate by Air-Argon ICP-AES

  3. 研究了SBS质量分数、环烷酸镍质量分数、nAl/nNi、反应氢气压力、反应温度等工艺条件对SBS加氢度的影响。

    The hydrogenation technological factors including the ρ _ SBS , w _ Ni , n _ Al / n _ Ni , hydrogen pressure and reaction temperature were researched to find the reaction condition of SBS hydrogenation .

  4. 本文简单介绍了环烷酸镍的用途,通过实验说明了环烷酸镍的制备路线及方法。

    The paper introduces the application of naphthenate nickel and explains the manufacturing way and method of naphthenate nickel through experiments .