固溶退火

gù róng tuì huǒ
  • solution annealing;solution treatment
固溶退火固溶退火
固溶退火[gù róng tuì huǒ]
  1. 样品材料包括:固溶退火的316不锈钢(316SA)、冷轧316不锈钢(316CW)和加钛的奥氏体不锈钢(Ti-mod.SS),HVEM的电子能量为1MeV。

    The specimen materials were solution annealed ( SA ) 316 stainless steel ( SS ), cold worked ( CW ) 316 SS and Ti-modified austenitic stainless steel ( Ti-mod . SS ) .

  2. 观察其显微组织和晶粒度,测定其显微硬度,分析了金相组织、晶粒度和硬度随固溶退火温度、保温时间、冷却速度的变化。

    The microstructure was observed and the grain size and Vickers hardness were measured , the changes of microstructure , grain size , hardness and solid solution annealing process were discussed .

  3. 冷变形退火后合金的内耗比固溶态高;退火温度升高,内耗增加。

    The internal friction of alloys annealed after cold deformation are higher than alloy in solid solution state . The internal friction increased with the increase of annealing temperatures .