  1. 油漆薄木贴面中密度纤维板TVOC释放量与薄木贴面中密度纤维板差异不大,甲醛释放量很少,苯系物相对较多。

    Less formaldehyde and more benzene released from spray MDF veneered veneer that had little difference in TVOC emission comparing with MDF veneered veneer .

  2. 试验结果表明:利用杉木积成材进行薄木贴面,工艺切实可行,奥古曼薄木贴面的较佳工艺参数为:热压温度100℃,热压压力10MPa,热压时间4min,涂胶量120gm2。

    The results show that veneer overlaying technology of China fir orient strand lumber is practical way and the better technology parameter is that hot press temperature 100 ? ℃, hot press pressure 1 0 ? MPa , hot press time 4 ?

  3. 水曲柳薄木贴面装饰板的表面化学处理

    Surface treatment with chemical agents for veneered plywood of Fraxinus mandshurica

  4. 工艺参数对硬枫薄木贴面杨木多层板表面质量的影响

    Effect of technology parameter on the surface guality of maple veneered wood

  5. 薄木贴面装饰板中水份的作用及控制

    Function and Control of Moisture in the Veneer-faced Decorative Board

  6. 用薄木贴面技术生产仿实木家具

    Making Wood Imitation Furniture with Method of Sheet Wood Overlaying

  7. 片状合成薄木贴面工艺及其质量缺陷的解决措施

    Flake Based Synthetic Veneer Overlaying Technology and Solutions to Its Quality Defects

  8. 薄木贴面工艺与技术

    Wood Veneer Overlaying Technology Overlaying Practice for Formed Plywood Components

  9. 中密度纤维板人造薄木贴面工艺的研究

    Study on artificial veneer overlaying process for medium density fiberboard

  10. 薄木贴面胶合板在室内设计中配色规律探析

    Exploration on Color Matching Rules of Veneer Overlaid Plywood in the Interior Design

  11. 薄木贴面工艺及贴面缺陷的预防措施

    Veneer Overlaying Technology and Precautionary Measures against Relevant Defects

  12. 采用正交试验法,探讨了杉木积成材薄木贴面的工艺过程。

    Veneer overlaying technology of China fir orient strand lumber is explored through orthogonal method .

  13. 本文阐述了薄木贴面装饰板生产中水份的调控措施,对生产具有一定的指导意义。

    This article has elucidated the regulatory and control measures of water in production-control of veneer-faced decorative board .

  14. 速生杉木为基材的水曲柳薄木贴面初步研究用薄木贴面技术生产仿实木家具

    Preliminary Studies on Facing Rapid-growth Cunninghamia lanceolata with Fraxinus mandshurica Thin Wood Making Wood Imitation Furniture with Method of Sheet Wood Overlaying

  15. 分析了薄木贴面工艺中,木皮起泡主要是由于表面不平、胶水固化程度和薄木含水率等原因所致。

    The bulges in veneering are mainly caused by the factors such as uneven surface , drying speed of glue , moisture content of veneer .

  16. 落叶松刨切薄木的研究贴面硅酸钙板

    Slicing veneer of Larch face-decorated calcium silicate board