结果表明:含汞10-4~10-6的酸性锌锰干电池,在300℃和系统残压为35~500Pa的条件下,真空处理3h,残渣含汞量可低于10-6。
Results show that under the condition of the total chamber pressure of 35-500 Pa , temperature of 300 ℃, the concentration of mercury in waste acid zinc-manganese cell can be decreased to a level lower than 10-6 after being treated for 3 h.