为消除LY12CZ铝合金激光焊接时焊缝中常见的气孔和裂纹缺陷,通过正交实验,优化了激光功率、扫描速度、保护气体流量等工艺参数,并采取适当的焊前预处理工艺。
Through orthogonal experiment , laser power , scanning rate and gas flow were optimized and pretreatment techniques were adopted to cancel pore and crack in laser weld of LY12CZ .
-
采用合理的焊前表面处理工艺、全熔透焊接可获得无气孔的焊缝。
The weld can performed free of porosity for full penetration weld when proper surface treatment processing prior to welding is employed .
-
PDC钻头焊前焊后处理工艺的试验研究
Study on the Treatment Technology before and after Welding of PDC Bit
-
用不同焊接方法,对坯料焊前作不同工艺处理,焊接成形时出现焊缝开裂,对其坯料母材及开裂焊缝作显微分析。
To do mycology analysis to the blank parent and its cracking weld for different procedure treatment to the blank before welding and occur weld crack during welding forming by different welding method .